Re: [MW:12717] RT Required for Pipe to WNFF

Hi,

As per UW-11 (a) (4), Nozzles exceeding 10NPS shall be radiographed, please find attached table for ease of reference:-
      
Regards
Manpreet Singh


From: Karthik <karthik6684@yahoo.com>
Sent: Wed, 19 Oct 2011 01:03:53
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: Re: [MW:12698] RT Required for Pipe to WNFF
Hi,
Please find below the extraction from ASME Sec.VIII,Div.1 - UW11.
UW-11 RADIOGRAPHIC AND ULTRASONIC
EXAMINATION
(a) Full Radiography. The following welded joints shall
be examined radiographically for their full length in the
manner prescribed in UW-51:
(1) all butt welds in the shell and heads of vessels
used to contain lethal substances [see UW-2(a)];
(2) all butt welds in vessels in which the nominal
thickness [see (g) below] at the welded joint exceeds 11⁄2
in. (38 mm), or exceeds the lesser thicknesses prescribed
in UCS-57, UNF-57, UHA-33, UCL-35, or UCL-36 for
the materials covered therein, or as otherwise prescribed
in UHT-57, ULW-51, ULW-52(d), ULW-54, or ULT-57;
however, except as required by UHT-57(a), Categories B
and C butt welds in nozzles and communicating chambers
that neither exceed NPS 10 (DN 250) nor 11⁄8 in. (29 mm)
wall thickness do not require any radiographic examination;
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

From: karthick enigoo <karthickenigoo@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, October 15, 2011 5:44 PM
Subject: [MW:12681] RT Required for Pipe to WNFF

Dear Friends,
 I need a clarification regarding, Pipe to Flange (Weld Neck). As per my drawing Design As per ASME Sec viii, Joint efficiency - 1, Radiography - Full & PWHT considered. Size of nozzles 80NB, 350NB & 500NB Sch 60. Radiography need to be done for all nozzles. 

--
Thanks & Regards,                                                    
D. Karthick
Ph.No: +91-9787300898

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...