[MW:12689] RE: 12682] CLAD MATERIALS -WELDING

Hi Pradip,

 

 

 

With Kind Regards,

 

S.Elumalai.


From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Sunday, October 16, 2011 3:51 PM
To: materials-welding@googlegroups.com
Cc: Sundaram Elumalai
Subject: RE: 12682] CLAD MATERIALS -WELDING

 

Hello Sundaram,

 

Would you be able attach a sketch of the weld joint indicating the sequences of  sequences of welding.

 

Thanks.

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist & Consultant

Ontario,Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sundaram Elumalai
Sent: Saturday, October 15, 2011 8:53 AM
To: materials-welding@googlegroups.com
Subject: [MW:12682] CLAD MATERIALS -WELDING

Hi experts,

 

We have the following Clad Pipe and we are preparing WPS /PQR to weld this SPOOL. As I know we need to use ERNiCrMo3 / E NiCrMo 3 ( if GTAW+SMAW) to Complete weld. But if any one is having experience with this, please advice whether we will go with

 

GTAW -  ER NiCrMo3  ( First four Passes- R/H/F1/F2)

SMAW – E7018-1  ( Balance Filling /Capping).

 

We have Pitting corrosion test as per ASTM G48 at 50 degree.

 

Pipe

NPS:10-Thk:45mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:15.88mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:45.5mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:53.5mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

 

 

 

With Kind Regards,

 

S.Elumalai.

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .