Re: [MW:11511] Welder's approval as per JIS but WPS is as per SEC IX

Dear Dave,
As you asked, according to my view if a WPS is qualified as per ASME
Section-IX. Welder will be acceptable on JIS specification. But it
must be check that in every case it follows the same or not.


On Wed, Jun 29, 2011 at 1:49 PM, shailesh dave <snd2988@yahoo.com> wrote:
> Dear Group members,
>
> Kindly let me know your views if welder can be accepted on JIS specification
> when WPS is qualified as per ASME Sec. IX. Can you prived me the applicable
> code which allow this.
>
> Regards,
>
> S.N.Dave
> Senior Inspection coordinator
> JGC gulf Inaternational
> Al Khobar
> Kingdom of Saudi Arabia.
> +966500184796
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
Regards
Ashish Yadav
Institute For Plasma Research

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...