Re: [MW:11498] Re: Welding in Poland

Mr.Raja,
Can you tel me why DNV cannot witness test and Approve PQR n WPQ as per ASME?
Muni

On Fri, Jun 24, 2011 at 1:29 PM, graja <agrajewski@gmail.com> wrote:
Hi,

as I know UDT and DNV Poland don't have ASME authorized inspector to
approve or coordinate welding acc. ASME, but TUV NORD, TUV Rheinland
or Lloyd Register in Poland have ASME authorized inspector so you can
ask them about ASME subject.

I work a little beat with ASME and if you don't have special
requirements about 3rd part you can approved PQR and WPQ by yourself.

sorry for my English, I have hope I help.

On Jun 23, 4:17 am, <vinit.deshpa...@akersolutions.com> wrote:
> Dear Experts,
>
> Need you your Help.
>
> One of our supplier has informed us that ''We cannot perform welding according to ASME because DNV Poland don't have accreditation for ASME''.
>
> As per my knowledge UDT is-Office of Technical Inspection working as an Inspection Body, as the Notified Body and the Recognized Third Party Organization as the Certification Body.
>
> Hence its a Inspection body only, my questions are as below,
>
> Is my understanding about UDT is correct?
>
> Can we do welding as per ASME in Poland?
>
> What are the options to be considered If we need to do welding in Poland according to ASME.
>
> Your early reply in this regard is appreciated
>
> Regards,
> Vinit Deshpande
> Aker Solutions
> Tel: +47-67826358
> Mobile: +47-45217814
> Email: Vinit.Deshpa...@akersolutions.com
>
> -
> This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this email and any attachments permanently from your system.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...