Friday, June 24, 2011

Re: [MW:11460] Voltage for GTAW electrode 2.4mm and 3.2mm

Dear,
 
Request you to find out SFA 5.12 PAGE NO. 312 Table A2 of ASME SEC IX, 2010 ED


 
On Thu, Apr 21, 2011 at 11:18 AM, Abuhanip bin Abdul <abuhanip@labuanship.com> wrote:

Dear sir.

               

                What is the voltage range qualified for the GTAW electrode 2.4mm with an amp range 120-175 and 3.2mm with an amp range 150-220?

I can't find it in the standard code. I need this for my pWPS..

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments: