Re: [MW:11454] Filler/Electrode for SA-312 TP310H to G-30 Hastelloy.

you can choose E/ERNiCrMo-11 or E/ERNiCrMo-10.
Interpass temperature should be maintained below (93ºC).

http://www.haynesintl.com/pdf/h2010.pdf
 
 
On Fri, Jun 24, 2011 at 3:13 PM, limesh M <limesh78@gmail.com> wrote:
Dear All,


What is the suitable GTAW filler wire and SMAW electrode to join SA-312 TP310H(UNS S31009) to G-30 Hastelloy?

What is the optimum interpass temperature range for this material?


Regards,

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...