The exothermic welding process is one in which the heat of welding is solely derived from chemical reactions. Therefore there is no “electrode”.
John
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of limesh M
Sent: Saturday, June 25, 2011 2:54 AM
To: Materials & Welding
Subject: [MW:11468] Exothermic Electrodes
Dear All,
Is there any electrodes called Exothermic Electrodes?