[MW:11489] RE: 11467] Minimun thickness requirement to carryout PWHT for CS

PWHT requirements are specified in the “book” or construction Code sections (i.e.  Section I, Section VIII, B31.1) or by customer specification.  Sc IX on tells one the requirements for qualifying welding or brazing procedures  and personnel working to them.  As such Sc IX does not specify a minimum thickness for PWHT than the applicable procedure thickness range based on PQR thickness.

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Venkateswaran
Sent: Saturday, June 25, 2011 2:15 AM
To: materials-welding@googlegroups.com
Subject: [MW:11467] Minimun thickness requirement to carryout PWHT for CS

 

Dear All

As per ASME Sec 8,what will be the minimun thickness requirement to carryout  PWHT for CS .Kl.refer me the page no/Table.

 

Regards,

K.Venkateswaran.

 

zero b footer 

Please consider the environment before printing this E-mail

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...