Dear All,
We did perform HT on our Dish ends (SS 316L, min thick 12mm) for our pressure vessels designed according to ASME VIII, Div 1 and NACE MR 0175.
The hardness values recorded by our supplier were between 24 and 38 HRC.Where the harndess limit stated by NACE MR 0175 Table A-2 is 22 HRC.
What can we do???
Is there any technical solution other than re-annealing???
Please share your ideas
Thanks
--
Meilleures salutations
Mokrani Lassaad
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
P Pensez environnement! N'imprimez ce mail que si c'est vraiment nƩcessaire
Please consider your environmental responsibility before printing this e-mail
This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments