Friday, June 24, 2011

[MW:11458] Re: PQR conversation -20 deg to -40 deg

Mr. Vimal,
You must qualify another PQR for this application. If you had
performed impact testing to -40°F in the beginning, the PQR could have
been used in applications where the MDMT/ CET is specified to be -20°F
without any repercussions. Hope this helps!

On Jun 23, 2:40 am, Vimal Mistry <vimal.mis...@suzlon.com> wrote:
> For ASME SEC-IX
>
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sudhakar kuppuswamy
> Sent: Thursday, June 23, 2011 10:26 AM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:11439] PQR conversation -20 deg to -40 deg
>
> dear Mr Vimal can you specify for which code ur working for. example ASME SEC 9 or AWS D1.1 etc..
>
> with regards,
> sudhakar.k..On Wed, Jun 22, 2011 at 3:38 AM, <vimal.mis...@suzlon.com<mailto:vimal.mis...@suzlon.com>> wrote:
>
> Dear All.
> I have PQR with -20 deg Impact & Values are 180 to 194 J Now I require
> PQR with -40deg Impact so can I go through same PQR with  -40deg
> Impact or I should qualify another.
>  If it's acceptable then which std/ spec. can be use as ref.
>
> Vimal
>
> --
> To post to this group, send email to materials-welding@googlegroups.com<mailto:materials-welding@googlegroups.co­m>
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com<mailto:materials-welding%2Bu­nsubscribe@googlegroups.com>
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
> With regards,
> Sudhakar.k
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> - Disclaimer--
>
> This email and any files transmitted with it are confidential and may be privileged or otherwise protected from disclosure and are intended solely for the use of the entity / individual to whom they are addressed. If you have received this email in error or If you are not the intended recipient, please notify the sender immediately by way of telephone or email and delete this message and any files transmitted from your system. Please note that any views presented in the email are solely those of the author and do not necessarily represent those of the organization. While all care has been taken to avoid viruses the recipient is advised to check this email and attachments for presence of viruses. The organization accepts no liability on this account.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...