Hi: 
 
I don´t now enough about IRIS technology but if you need to inspect tubing of boilers or heat exchangers you can use ET or RPA technologies, Recently I use RPA with excellent results, all depends of the conditions of you industrial process. You will find more information about RPA in the next web page: www.acousticeye.com
 
Best Regards 
 
Jorge Clemente
 
 
De: materials-welding@googlegroups.com
Para: materials-welding@googlegroups.com
Cc:
Fecha: Mon, 18 Apr 2011 21:21:12 -0700 (PDT)
Asunto: [MW:10731] IRIS inspection

> Dear experts,
>  
>                 What is IRIS? where does this used? What is the limitations? Is this applicable only to inspect in CS tubing of boilers or both CS & SS.
>  
> Thanks in advance.
>  
> Regards
> Ilangkumaran

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...