Hi,
Please refer Table 5 of ASTM A312-06. It is very clear.
Paulose John
On Sun, Apr 17, 2011 at 6:15 PM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
for Gtaw, either ER321 Or ER347 shall be used but for SMAW only E347 is to be used because if we use E321, there will be loss of Titanium alloying loss in arc streampandithanOn Fri, Apr 15, 2011 at 3:10 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,--
In our project we have to weld Austenetic SS grade 321H full GTAW, we used ER 308 gtaw rod filler metal, one collegue say that we must use ER 347. is it true ? use ER 308 is not compatible with these grade ?
Please help me
Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment