Re: [MW:10696] qualified thickness range

With impact test thickness range is t/2 to t+6  means (8/2mm =4mm )   to  (8+6=14mm)
 
Means with Impact test thk range is 4m to 14mm
Without impact test thk range is 4.8mm to 16mm is currect
 
Saji Jos P
AbuDhabi
00971 56 6742779


From: raja sekhar <raj.inspection@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sun, 17 April, 2011 8:01:07 AM
Subject: Re: [MW:10693] qualified thickness range

Yes,
I think you are refring to same supporting PQR only for the both thickness ranges.
 
For E.g, If you have qualified a PQR with a thk of 8 mm with impact test.
 
Your qualification ranges in the WPS will be
 
8 to 16 mm (WIth Impact test)
5 to 16 mm (Without Impact test)
 
You can write both the reading in the WPS.
 
Hope this will clarify.
 
Cheers!
 
Raj

On Thu, Apr 14, 2011 at 7:57 AM, Ali Asghari <asghariali@rocketmail.com> wrote:
Dear all
Is it possible a WPS issued that have two qualified thickness ranges?( one of them supported by a PQR that impact tested and another range with ignorance of the CVN results acc to ASME IX)
Regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...