Saturday, April 2, 2011

Re: [MW:10580] RE: 10463] Backing

Mr Karthik
 see the clarification, it is a back weld(double side), and i go with john
 
Pandithan, AWS-CWI,CSWIP 3.1
In-Charge/Welding Technology
Cethar Vessels Ltd
Trichy

On Wed, Mar 23, 2011 at 8:11 PM, John Henning <jhenning@deltak.com> wrote:

YES – it is welding with backing.

 

See QW-402.4, non-essential variable for both SMAW and GMAW and an essential variable for welder performance qualification for both processes per QW-416.

 

"QW-402.4  The deletion or the backing in single  welded groove welds.  Double welded groove welds are considered welding with backing."

 

John

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Venkateswaran
Sent: Wednesday, March 23, 2011 4:11 AM
To: materials-welding@googlegroups.com
Subject: [MW:10463] Backing

 

 

As per ASME SEC IX ,we qualified PQR(SMAW/GMAW process) with 8mm/10 mm thickness plate full penetration welding( Root Land:1mm to 1.5 mm) as root ,hot and cap welding and then back/root side of plate was grounded(approx 2mm) to sound metal and one pass of cap welding was done in root side.

My question is whether is method is considered as welding with backing or with out backing it is considered as backing. how?

 

 

 

Regards,

 

kvr

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...