RE: [MW:10575] DPT for Structural welding

no need to do DPT for rootrun BUT IF BACKGOUGING is consider  then DPT required but 10% DPT should be done for final weld.

Regard,
Narendra P. Makode,
Production Engineer,
Wheels India Ltd.
Heavy Engineering Ltd. Deoli,Wardha.

M : 09049993668
Email:-
narendra_pmakode@yahoo.co.in


--- On Fri, 1/4/11, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: RE: [MW:10574] DPT for Structural welding
To: "'materials-welding@googlegroups.com'" <materials-welding@googlegroups.com>
Date: Friday, 1 April, 2011, 5:11 PM

None by code, it shall be specified by the designer

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Feroz Mohammed
Sent: Friday, April 01, 2011 5:05 PM
To: materials-welding@googlegroups.com
Subject: [MW:10573] DPT for Structural welding

 

Dear All

 

Can any body tell me if it is required to do DPT for root run & after final welding in structural steel. If yes how much percentage

 

CODE: AWS D1.1

--

Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I

LANCO Infratech Ltd.

È : +91 9650490097
 

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...