Thursday, February 24, 2011

Re: [MW:9998] welding of GI ( galvanized iron) material

Welding Galvaised steel is similar to welding any carbon steel. One option to reduce health Hazard, the Zinc coating can be removed from the weld joint and surronding area by grinding or using Emery paper. Then carry out the welding.

J.GERALD JAYAKUMAR
00919344954677
 


--- On Wed, 2/23/11, Manindra Singh <hellmanya@in.com> wrote:

From: Manindra Singh <hellmanya@in.com>
Subject: [MW:9981] welding of GI ( galvanized iron) material
To: materials-welding@googlegroups.com
Date: Wednesday, February 23, 2011, 8:16 AM


Dear colleagues
Please let me know about the details of welding of GI ( galvanized iron) material & its pros and cons.
M P Singh
Inspection Engineer


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...