He will not disqualified untill he cross the perecentaage limit of
rejection as per project spec or code ...

Please refer related documents ...

I think he should able to do 2 weld joints W.r.t penalty....

Suresh

On 2/24/11, Shaunak Upadhyay <shanupadhyay@gmail.com> wrote:
> Dear All,
>
> If one 6G Qualified welder welds one joint and after rt test that
> joint full repair, than can we disqualify that welder?
>
> Is there any code or specification for this issue.
>
> Please give your suggestion.
>
> Regards,
> Shaunak Upadhyay.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...