Re: [MW:9989] Elongation Percentage for Dish End / Calculation

Dear Vino

Pls. refer UCS 79 & UG 79 of sec VIII div 1 for fiber elongation

What is the material and what is the dimensions, type of head .....


cheers
MM

On Wed, Feb 23, 2011 at 1:55 PM, Vino Varghese <vinopvarghese@gmail.com> wrote:
Dear Friends/Advisers,
 
Design: ASME Sec VIII, Div 1.
Material & Thickness: SA 516 Gr.70 & 30 mm.
 
1. Please provide a method to calculate Elongation % after Forming(Hot/Cold) for Pressure Vessel Dish End.(Ellipsidol 2:1)
2. What should be the thickness selection to achieve 30 mm final thickness?
3. How to ensure that Materials Fibre Elongation is less that 5%? This is required to avoid SSC Test with regard to NACE requirement.
 
Hope to see as usual co-operation.
 
Regards
Vino P Varghese
Doha-Qatar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...