Re: [MW:9974] LTCS

LTCS is low temperature carbon steel which can be used at low temperatures according to the applicable specification.
Yes is the answer to your query if impact tested at the required temperature.

 
J.GERALD JAYAKUMAR
00919344954677
 


--- On Tue, 2/22/11, ramu ramalingam <ramu.srivi@gmail.com> wrote:

From: ramu ramalingam <ramu.srivi@gmail.com>
Subject: Re: [MW:9972] LTCS
To: materials-welding@googlegroups.com
Date: Tuesday, February 22, 2011, 7:37 AM

what is the difference between CS & LTCS material.some time material heat numbers were both in one manufacturing and chemical and mechanical both are same in both materials.but one had impacted.Is it ok? Material can be used in production?
Ramu

On Thu, Jan 27, 2011 at 3:23 PM, Karthik <karthik6684@yahoo.com> wrote:
Low Temperature Carbon Steel (LTCS)..This material used for Low temperature application on pressure vessels etc.,

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Thu, 1/27/11, Pardeep <fab_qc@isgec.com> wrote:

From: Pardeep <fab_qc@isgec.com>
Subject: [MW:9522] LTCS Date: Thursday, January 27, 2011, 3:55 PM


Can any body tell me what is LTCS and its full form.
 

 (Before Printing, Think about the environment, every 3000 A4 paper costs 1 tree. Please DO NOT print unless you really need it. This will preserve trees on planet earth.)

 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of muthu barathi
Sent: Thursday, January 27, 2011 1:35 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9517] CS in place of LTCS
 
hi

If cooling water , then the CS pipe tested with impact and the
temperature should be more than your fluid temperature . if the fluid
temperature is (-))10 deg C then your base metal should be at least (-)
20 deg C. in this way your CS is there then you may replace or you have
to go for LTCS.


On Thu, 27 Jan 2011 12:39:26 +0530 wrote
>Can we replace LTCS with CS if temperature minimum expexted is

-20DegC,process fluid;Coolwing water???



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

Image removed by sender.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...