Dear sir,

You can get good quality of weldments in 4G position as well, pls go ahead
with your PQR/WPS

Thanks & Regards,

K. Babu

----- Original Message -----
From: "haseeb ph" <haseebph@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Monday, February 21, 2011 7:06 PM
Subject: [MW:9958] Re: FCAW -4G -WPS & WPQ is possible or not ? Most urgent


hello sir,

I have a doubt about the quality of the weld when we are using FCAW in
4G position.I think it is not a good idea to use fcaw in 4g position
How about you sir

On Feb 20, 11:18 am, "K.Babu" <kbabu...@gmail.com> wrote:
> Hi Srinivas,
>
> Very well possible.
>
> On Sat, Feb 19, 2011 at 9:01 PM, Srinivas Engr
> <srinivas.gmsr...@gmail.com>wrote:
>
>
>
>
>
>
>
>
>
> > Dear All.
>
> > pl clear me on tat.
> > Can We Qualidy WPS & WPQ in FCAW Process in 4G position is possible or
> > not?
> > Code is AWS D1.1.
> > Is any practical problem in tat?
> > Its urgent/
>
> > Thanks & Regards
>
> > Srinivas
>
> > --
> > To post to this group, send email to materials-welding@googlegroups.com
> > To unsubscribe from this group, send email to
> > materials-welding+unsubscribe@googlegroups.com
> > For more options, visit this group's bolg at
> >http://materials-welding.blogspot.com/
> > The views expressed/exchnaged in this group are members personel views
> > and
> > meant for educational purposes only, Users must take their own decisions
> > w.r.t. applicable code/standard/contract documents.
>
> --
> Thanks & regards,
>
> K.Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...