Re: [MW:10059] In-service welding qualification of SS pipe line

Hii
First you need to specify whats construction code you are using ...

I think particularly there is no code for In Service welding WQT
test,Generally we arre following ASME SECTION IX .

Suresh

On 2/28/11, joshi jaydeep <jaydeep.p.joshi@gmail.com> wrote:
> Dear all,
>
> As per the scope of API 1104, It is restricted to be used for CS and LAS
> material.
>
> Which code is to be followed for In-service welding qualification of SS pipe
> line.
>
>
>
> *Jaydeep Joshi | Welding Engineer, TDW India Limited*
>
> Plot No 16 | Phase –III | Alindra – Savli G.I.D.C | Taluka : Savli |
> Vadodara – *391 775*
>
> *Board* : +91-2667- 619900 | *Fax *: +91- 2667- 619501| *Extension : 7845*
>
> E-Mail : jaydeep.joshi@tdwilliamson.com <samyak.sahani@tdwilliamson.com> |
> *www.tdwilliamson.com*
>
> Cell: +91 9978959626
>
> P *Before printing, Think about ENVIRONMENTAL responsibility*
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...