Monday, February 28, 2011

Re: [MW:10055] excess penetration for butt weld joints

Dear Mr.Abhay,

Have you refer the trailing mail table ASME B 31.3 ,342.3.2 table then you will ask the next question.

I think just like feeding Everything is not good refer it for internal protrusion or excess penetration limits.

Regrds,

PSR

On 28 February 2011 18:01, Abhonkar, Abhay (NAR) <AAbhonkar@dresser-rand.com> wrote:

My question is on excess penetration for root and not for excess reinforcement.

Generally it is to be minimum for smooth flow of media but I want to know acceptance standard from ASME sec IX or B 31.3.

 

 

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Fitria Rahman
Sent: Sunday, February 27, 2011 1:00 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10036] excess penetration for butt weld joints

 

Please refer to table 341.3.2 ASME B31.3 for criteria of height of reinforcement

2011/2/24 Abhonkar, Abhay (NAR) <AAbhonkar@dresser-rand.com>

What is the acceptable excess penetration as per the B31.3 or ASME sec?

Whether we can consider the same as defect or discontinuity?

Pl advise.

 

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...