Saturday, February 26, 2011

Re: [MW:10024] Tank Peaking/Banding Issue, API 650

Dear Sir,
 
Thank you very much for replying, but problem is that API 650 by itself refering to mentioned standard like ASTM A 6M etc.
 
Please advice,
 
Abdul Wahab

On Sat, Feb 26, 2011 at 3:24 PM, Suresh <bobsuresh24@gmail.com> wrote:
Hii Abdul ,

You should follow API 650 for tank consrtuction , not ASME code .

In my best of my knowledge , you need to refer to API 650 and follow
tolarances which was mentioned in API 650 .

Thank you

Suresh

On 2/26/11, Abdul Wahab <awengineer@gmail.com> wrote:
> Dear All,
>
> I am Abdul Wahab working in KSA as QA/QC Inspector, I have an issue
> which is confusioning me. Below there is copy of Paragraph of API 650.
> Plumbness, peaking, banding & flat spot discussed in this & tolerances
> are provided but along with tolerance of API 650, also refering to
> ASTM standards, those standards have tolerances aproximately a double
> values as compared to API 650 Tolerances. Do we need to follow those
> as ASTM is not a tank construction code but provide guidance about
> matrial manufacturing,testing & handling etc.
>
> We have Banding Value for 6 mm Plate of 13 mm max,  can we consider a
> dent as a banding problem in tank shell.
>
> Please see below & advice.
>
> 7.5.2 Plumbness
>
> a. The maximum out-of-plumbness of the top of the shell relative to
> the bottom of the shell shall not exceed 1/200 of the total
> tank height. The out-of-plumbness in one shell course shall not exceed
> the permissible variations for flatness and waviness as
> specified in ASTM A 6M/A 6, ASTM A 20M/A 20, or ASTM A 480M/A 480,
> whichever is applicable.
>
>
>
> 7.5.4 Local Deviations
>
> c. Flat spots measured in the vertical plane shall not exceed the
> appropriate plate flatness and waviness requirements given in
> 7.5.2.
>
> If there is any confusion to understand, please ask.
>
>
> Abdul Wahab
> Mechanical Inspector
> KSA
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...