Hai
 
first of all, SA 106 Gr.B Material above 19mm only we need to do the PWHT. at what specification you are following the PWHT for sch40 pipes.
 
in case of your specification, you have to do PWHT, then you have to go for the new modified joint also. then go for RT.
 
generally, modified weld also must do the similar way for other joints. RT also should take.
 
 
 
 
On Fri, Feb 25, 2011 at 10:02 AM, Abhonkar, Abhay (NAR) <AAbhonkar@dresser-rand.com> wrote:

Dear Sir,

This is case for discussion.

Let us assume that piping for SA106 Gr B pipes are fabricated and radiographed and found OK. Then as per the requirement, next stage is Post weld heat treatment.

Size of the piping is vary between 1 inch sch 80 and extends upto 10 inch sch 40 CS SA106 Gr b NACE material.

 

Now if one completed the PWHT cycle and during mounting of the piping it seems that without doing the re cutting and rewelding it will not fit then, how we should go forward,

 

1)       Can piping accepted by means of radiograph after rewelding and if RT OK then we can go ahead for final hydro test without PWHT.

2)       One has to do again PWHT for that modified joint.

3)       What is AEME verdict about that?

4)       Whether UCS – 56 is mentioned about that, as it will seems that code mentioned about repair weld only and not for new weld after modification.

 

Pl have your views on above.

 

 

Regards,

Abhay

Ext 448

 

IMPORTANT NOTICE:
This email may be confidential, may be legally privileged, and is for the intended recipient only. Unauthorized access, disclosure, copying, distribution, or reliance on any of it by anyone else is prohibited and may be a criminal offense. Please delete if obtained in error and email confirmation to the sender.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,

Rengaraja.T

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...