[MW:10021] Re: TECHNICAL CLARIFICATION 1- WPS AND PQR

Dear Mr. Moin,

I agree fully with mr. James Gerald regarding his answer for interpass
temperature and disagree with some others. ASME section IX QW492 gives
the following definitions for the Interpass Temperature:

QW492:interpass temperature:
the highest temperature in the weld
joint immediately prior to welding, or in the case of multiple
pass welds, the highest temperature in the section of
the previously deposited weld metal, immediately before
the next pass is started.

So interpass temperature is not related to single run welding and also
doesn't need to be monitored during welding of single runs because
definition clearly says "prior to welding" instead of "during
welding".

Best Regards

Herman Pieper

On 24 feb, 05:42, james gerald <gerry_...@yahoo.com> wrote:
> Moin,
>  
> Yes, It is mandatory to mention Weld Metal thickness in the WPS for each applicable process say GMAW and SAW. During your PQR qualification, in the Run-out sheet you can measure and record the bead Height for each pass and calculate the exact thickess for each process. Then the Qualified thickness is 2t according to QW451.1 which can be checked and measured in the actual production Joint.
>  
> It is not required to mention the Lot number of the Flux/wire in the WPS. It can be controlled via another document giving the list of Lot numbers to be used for any particular job which requires special testing or control. But the Consumable certificate for the particular lot shall be available with the Welding Engineer and confimed its compliance according to ASME Sec.IIC + required additional testing. One reason why a separate document is used instead of mentioning in the WPS is if the Lot numbers are many, then there may be space constriction.
>  
> Interpass temperature is the temperature between each pass. Since it is a Single pass, no Interpass temperature is applicable.
>
> J.GERALD JAYAKUMAR
> 00919344954677
>  
>
> --- On Wed, 2/23/11, Moin - QC <Syed.M...@gerabgroup.com> wrote:
>
> From: Moin - QC <Syed.M...@gerabgroup.com>
> Subject: [MW:9984] TECHNICAL CLARIFICATION 1- WPS AND PQR
> To: materials-welding@googlegroups.com
> Date: Wednesday, February 23, 2011, 11:30 AM
>
> Dear friends,
>
> I have few question related to WPS, I am trying to check whether it complies to XI though I am not  CSWIP certified or a welding engineer, appreciate if you could provide some information to me on the  following
> 1-      Is it mandatory to mention the qualified weld metal thickness on WPS, if yes  what should be qualified weld metal thickness for a test coupon 9 mm thick and welded by GMAW and SAW process , should it be 2t as per table QW 451.1?  How to find '' t'' before doping welding?
>
> 2-      Is it mandatory to mention the lot number of flux& wire on the WPS, if No could you please provide me reason?
>
> 3-      My understanding is if the welding is single pass than interpass temperature does not come into picture is it true?
>
> Thanks & Regards
> Syed Moin                               
>
> ______________________________________________________
> CONFIDENTIALITY NOTICE: This electronic mail transmission may contain information that is confidential, privileged, proprietary, or otherwise legally exempt from disclosure and is intended only for the use of the recipient named above. We do not waive confidentiality in the event this mail was transmitted wrongly. If you have received this communication in error, and are not the intended recipient, you are hereby notified that you are prohibited from reading, printing, copying, or disseminating this message, any part of it, or any of the attachments it may carry. If you have received this message in error, please destroy all electronic and paper copies and notify the sender immediately of the inadvertent transmission. We would like to advise you that we would not waive any of our privilege for taking action against you in the event the confidentiality of this message has been compromised. Thank you for your cooperation
> ________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please visithttp://www.messagelabs.com/email
> ______________________________________________________________________
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...