Thursday, January 27, 2011

Re: Re: [MW:9521] CS in place of LTCS

@ CS in place of LTCS
 
i mean to know if we are taking well care of low temperature/using impact tested CS ,then CS would be a better metallurgy than LTCS or not because LTCS is having (Cr+Ni) ,certainly having better properies than CS in terms of corrosion????
 
Any experience of repl;acing LTCS tubes with CS tubes in heat exchanegrs is appreciated.
 
 
regards.


On Thu, Jan 27, 2011 at 1:42 PM, muthu barathi <muthu_barathi@rediffmail.com> wrote:


Hi,

SA 516 Grades all comes under (SPECIFICATION FOR PRESSURE VESSEL
PLATES,
CARBON STEEL, FOR MODERATE- AND LOWER TEMPERATURE SERVICE)

while ordering you have to mention the requirement in supplementary
S5. Charpy V-Notch Impact Test,then you will get LTCS.




On Thu, 27 Jan 2011 12:50:01 +0530 wrote

>
Dear All,

Can anybody tell me theMaterial A516Gr. 55 is C.S orLTCS?
Thank's,
>

>
>
>REMEMBER ME IN UR PRAYERS !
>*******(¨`·.·´¨) (¨`·.·´¨)********
>********`·.¸(¨`·.·´¨)..·´*********
>*********** `·.¸.·´************

>Best Regards,
>Ayaz Merhmood
>FEDC Dept.
>I-G-D HABSHAN-5 PROJECT
>DESCON ENGINEERING (UAE)
>Mobile :
+971-50-1926232
>www.descon.com.pk

>

>


From: yogesh
>To: Materials & Welding
>Sent: Thu, January 27, 2011 10:22:53 AM
>Subject: [MW:9512] CS in place of LTCS
>
>Can we replace LTCS with CS if temperature minimum expexted is
>-20DegC,process fluid;Coolwing water???
>
>--
>To post to this group, send email to materials-
welding@googlegroups.com
>To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...