Dear Asim,

Please provide the following,

1.Tube Sheet material and thickness.
2.Tube to tube sheet weld joint configuration.
3.Your shell side service environment and material.

Assuming your shell side process fluid is corrosive, which will has access to the root of the tube to tube sheet weld joint, such a situation will call for purging the shell side.

Also use a suitable filler material when welding the tube to tube sheet weld joint, do not weld it without filler material.


Regards,


A.Praveen
Muscat

--- On Sat, 1/29/11, ASIM MUNIR <asimmunir.002@gmail.com> wrote:

> From: ASIM MUNIR <asimmunir.002@gmail.com>
> Subject: [MW:9547] Purging of fillet weld
> To: materials-welding@googlegroups.com
> Date: Saturday, January 29, 2011, 1:20 PM
> Dear Experts,
> Can anybody please guide about purging of fillet welds of
> tube to tube
> sheet of a heat exchanger. Please conceder the followings
> 1- Material is duplex
> 2- Thickness of tube is 1.6mm
>
> is the purging mandatory for tube to tube sheet weld
>
> Thanks in advance.
> --
> Regards,
> MUHAMMAD ASIM MUNIR
> QA/QC INSPECTOR
> MOODY INT.
> CELL #+923007815592
>        
>    +971566230102
>
> "QUALITY IS MORE IMPORTANT THAN QUANTITY"
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...