Dear Mr.Anil Varma
 
We are baking the flux at 300 deg c for 2 hrs.  For 3.2 mm wire we are using the current range of 425-500 Amps
 
Regards
 
Rinshad A

On Thu, Jan 27, 2011 at 12:24 PM, Arc Welding Company <arcweldingcom@gmail.com> wrote:

Dear sir,

Hope  your are baking the flux properly. Do you face slag removal difficulty even after proper baking of flux? Excessive currents is also responsible for slag removal difficulty.

Regards,

For arc welding company,

Anil verma

9999200148

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...