Sunday, January 30, 2011

Re: [MW:9563] diameter and thickness limit

Dear Hussain ,
 

As per QW 452.3, upper diameter limit is unlimited.

That means , you can go for unlimited Dia which has no limit .....

As per QW452.1b, for test coupon 13 mm and above, qualification limit is 'maximum to be welded.'

That means  how much you can able to weld to prove  to  make good sound welds .....,this criteria is only for thickness ........not Diameter .

Thank you

Suresh

 

 



On Sun, Jan 30, 2011 at 6:11 PM, Ahmed Husain <ahmraha@yahoo.com> wrote:

Dear All,

My query is in regard to welder performance qualification diameter and thickness limit as per ASME Sec IX

As per QW 452.3, upper diameter limit is unlimited.

As per QW452.1b, for test coupon 13 mm and above, qualification limit is 'maximum to be welded.'

I would like to know that this "maximum to be welded" is to be considered same as unlimited or there is any limit.

With regards,

A.Husain


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...