Dear all
I reviewed a Material certificate for Duplex SS, Plate A240 UNS S31803 and found Nitrogen content .08 – 0.2% as required by ASME sec II part A is not at all mentioned in the certificate. As vessels are fabricated and welded I issued a NCR to manufacturer.
Vessel manufacturer are going to ask Mill about this.
1) My question is how come a Mill certificate misses an essential element of composition required by the code? If the Mill comes with a reply that it is a clerical error to miss the Nitrogen content, and re-issue a certificate, can we accept it as genuine?
2) Is nitrogen content can be analysed by PMI or any other analyzing method in a lab test. Because the vessel fabricator say they are going to do lab test, for this.
Please share your experiences and opinion about this.
Thanks
Murugesan
--To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments