Dear all,
 
We are going to make SMAW+SAW PQR With following
 
SMAW-E7018 
 
Base metal SA516 Gr.70 (P nr.1,Gr.2)
 
Flux-Filler-ESAB OK Autorod 12.22 (EM12K) ESAB OK Flux 10.62 (F7A8-EM12K)
 
slag removal for the hot pass is seams to be very difficult , we are not having experiences in SAW process..
 
 what will be the reason ?
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...