Dear Sir,
                 I would like to know that base on previous projects qualified PQR says that Argon Gas purity 99.90% but requirement is 99.996%.Main things is gas is essential variable So I want to use this PQR.During preparation wps, can i  purpose argon purity is 99.996%
 
Pl suggestion me
 
Regards
Bijaya



--