Hi
There is no expiry date for the consumables.
You can use the consumables , as long as the condition is good.
May be you need to get approvals for the batch's if the approval is expired for the concerned consumables lot
Thanks & Regards,
K. Babu
----- Original Message -----
From: SureshSent: Monday, January 31, 2011 1:15 PMSubject: Re: [MW:9575] Expiry period for SMAW consumable-regHiiGenerally Consumable expiry date is up to 2 monsoons,or Manufacturer should specify in Batch/Lot certificate .On Mon, Jan 31, 2011 at 9:35 AM, Pandiaraj <pandi.kali@gmail.com> wrote:
Dear Experts,
generally what is expiry period for SMAw consumables (Flux coated) dose ASME Sec II-C refers regarding this, if so please refer which class.in the consumable wraper only manufactured date is given but not the expiry date.
Thanks & Regards,
K.Pandiarajan.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Best Regards,
Suresh
Mobile No: 91-92 92 905 905
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments