Hi
 
The elongation requirement is very stringent, it is very difficult to meet 46%, you have consult with the specific consumable suppliers to get 46%
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
Sent: Thursday, January 27, 2011 4:36 PM
Subject: [MW:9523] Requirement of suitable welding consumables SAW and SMAW

Hi Friends,

Let me get your expertise of selection of welding consumables in this
regard.

The base material Chemical properties as given under (%):

C - 0.066
Si - 0.26
Mn - 1.55
P - 0.014
S - 0.004
Al - 0.046
Cr - 0.186
Ni - 0.015
Mo - 0.002
Cu - 0.020
V - 0.057
Nb - 0.065
Ti - 0.020
N - 0.007
B - 0.00025
Ca - 0.0025
CE - 0.371

MECHANICAL PROPERTIES
YIELD STRENGTH - 516 MPa
TENSILE STRENGTH - 625 MPa.
ELONG % - 46
IMOPACT - (-) 10 DEGREE C - 250 JOULES

NOW PLEASE TELL ME, WHICH ELECTRODE FOR SMAW (BRAMDS ESAB, OERLIKON)
AND SAW - FLUX AND WIRE WILL SUIT AND PASS PQR TEST FOR PREPARATION OF
WPS?

PLEASE HELP.
THANKING YOU.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...