[MW:0] RE: Cr. % Changing in heat Treatment

What is the %Cr you are getting? Normally this various is possible even if you take at different locations, and not because of HT . +/-10% variation over the specification requirement can be accepted in PMI. If you want precise readings try other methods.

 

From: israr ahmed [mailto:ahmedisrar.nm@gmail.com]
Sent: Sunday, January 30, 2011 12:30 PM
To:
Subject: Cr. % Changing in heat Treatment

 

Dear Sir,

 

I am Israr Ahmed working as a surveyor in one of the co. in mumbai,

Recently I witnessed a PMI test on Raw Material EN10083-34CrMoNi6.I was getting the result as per the requirements.

Now after machining and Heat Treatment of the same material I witnessed the PMI. The cr. percentage is getting down by 0.1percentage.

Both Time PMI done by a same Lab.

 

Could you pls guide me what may be the reason.

 

Regards 
Israr Ahmed Noor Mohammed
+919930308261