The base material Chemical properties as given under (%):

C - 0.066
Si - 0.26
Mn - 1.55
P - 0.014
S - 0.004
Al - 0.046
Cr - 0.186
Ni - 0.015
Mo - 0.002
Cu - 0.020
V - 0.057
Nb - 0.065
Ti - 0.020
N - 0.007
B - 0.00025
Ca - 0.0025
CE - 0.371

MECHANICAL PROPERTIES
YIELD STRENGTH - 516 MPa
TENSILE STRENGTH - 625 MPa.
ELONG % - 46
IMOPACT - (-) 10 DEGREE C - 250 JOULES

NOW PLEASE TELL ME, WHICH ELECTRODE FOR SMAW (BRAMDS ESAB, OERLIKON)
AND SAW - FLUX AND WIRE WILL SUIT AND PASS PQR TEST FOR PREPARATION OF
WPS?

PLEASE HELP.
THANKING YOU.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...