Monday, January 31, 2011

[MW:9593] Re: Hoe to select Flange's rating and class

Refer ASME 16.5,
Based on material, select material group & pressure temperature rating
table. Rating & class can be determined based on design temperatre &
pressure.


On Jan 31, 10:11 am, Saamy <krishnasamy1...@gmail.com> wrote:
> Dear All!
> Could you explain me how to select flange ratings and class against
> service, temp, and pressure?
>
> Thanks!
>
> Saamy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...