Dear Saamy,
 

1- Flange material shall be selected based on service conditions (fluid properties such as corrosiveness, temperature, hydrogen contents,...).

2- Based on design pressure, design temperature and material of construction the flange rating shall be selected according to pressure/temperature rating tables of ASME b16.5.

Based on my long experience on this matter I found that working with pressure/temperature rating tables of ASME b16.5 is not so easy and accurate. So I converted these tables to the graphs which is in attached as a pdf file for your convenience.

 

Hope it will be useful for you.

 

Regards,

Karandish



From: muthu barathi <muthu_barathi@rediffmail.com>
To: materials-welding@googlegroups.com
Sent: Mon, 31 January, 2011 1:32:49 PM
Subject: Re: [MW:9592] Hoe to select Flange's rating and class

Hi,
You have to refer your LDT (Line designation table) and P & ID (Process
instrument diagram).



On Mon, 31 Jan 2011 10:49:05 +0530 wrote
>Dear All!

Could you explain me how to select flange ratings and class against

service, temp, and pressure?



Thanks!



Saamy



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-
welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...