Dear Mr.Azaz,

SA 516 Gr.65 is low temperature carbon steel material used for moderate and lower temperature service and its having impact test properties.

Regards,

Thiru.



--- On Thu, 27/1/11, Ayaz Mahmood <tigerheart_ayaz@yahoo.com> wrote:

From: Ayaz Mahmood <tigerheart_ayaz@yahoo.com>
Subject: Re: [MW:9513] CS in place of LTCS
To: materials-welding@googlegroups.com
Date: Thursday, 27 January, 2011, 12:30 PM

Dear All,
 
          Can anybody tell me the Material A516 Gr. 55 is C.S or LTCS?
Thank's,
 




REMEMBER ME IN UR PRAYERS !
*******(¨`·.·´¨) (¨`·.·´¨)********
********`·.¸(¨`·.·´¨)..·´*********
*********** `·.¸.·´************

                                  
Best Regards,
Ayaz Merhmood
FEDC Dept.
I-G-D HABSHAN-5 PROJECT
DESCON ENGINEERING
(UAE)
Mobile : +971-50-1926232

www.descon.com.pk




From: yogesh <yogeshandpini@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thu, January 27, 2011 10:22:53 AM
Subject: [MW:9512] CS in place of LTCS

Can we replace LTCS with CS if temperature minimum expexted is
-20DegC,process fluid;Coolwing water???

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...