Re: [MW:9563] diameter and thickness limit

Dear Ahmed,

If any welder weld a single process (either SMAW or GTAW) with 13mm (with min. 3 or more passes) and above then one is qualified to weld in that process for unlimited thickness, if less than 13mm then qualified thickness is (2*t) where t is weld metal thickness.

"Max. to be welded" is corelated to qualified thickness in WPS, suppose if you qualified welder on 13mm weld metal thickness with SAW process and have a WPS qualified for 3" thickness in the same process, then welder can weld upto 3" thickness in SAW process. 


Regards
Manpreet Singh





On Sun, 30 Jan 2011 18:28:32 +0530 Ahmed Husain wrote
>

Dear All,

My query is in regard towelder performance qualification diameter and thickness limit as per ASME Sec IX

As per QW 452.3, upper diameter limit is unlimited.

As per QW452.1b, for test coupon 13 mm and above, qualification limit is 'maximum to be welded.'

I would like to know that this "maximum to be welded" is to be considered same as unlimited or there is any limit.

With regards,

A.Husain


>

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...