IS 2062 is an unlisted material

SS 410 will under P number 6 ( refer table QW/QB 422)

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of puneet takiar
Sent: Sunday, January 30, 2011 8:04 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9565] P1 no Range

 

Hello!

Can anybody tell me in which P. no IS 2062 grade A and SS 410 will fall and how to search in ASME sex IX table.