I need the information on the technical base not on any code base, wht
the code says like plus or minus.
I am not going to mention the things in WPS or PQR.
So my question is if I want to know the effect of heat input, which
amount of heat input I shall consider??
every single pass or sum of all heat input.
Regards
Sandeep Kumar
On Jan 28, 1:15 pm, "Pablo J Acelajado" <pjacelaj...@npc.com.sa>
wrote:
> January 28, 2011
>
> Hello!
>
> You need to show the individual Heat input of each pass and also
> indicate the sum or total Heat input.
>
> Thanks & best regards.
>
> PJA
>
> ________________________________
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of manpreet
> Sent: Friday, January 28, 2011 9:55 AM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:9538] heat input calculation in welding
>
> Dear Sandeep,
>
> As stated by you that "every pass has its effect on base metal", Your
> PQR shall include heat input for each pass and WPS to be written with
> Heat Input for each pass, as per QW-409.1, any increase in heat input
> for each pass will require requalification.
>
> Heat input shall be calculated with QW-409.1 (a) and (b), if with any of
> these methods Heat Input is increased, you need to requalify the WPS,
> that's why max. heat input value is written for WPS.
>
> Regards
> Manpreet Singh
>
> On Fri, 28 Jan 2011 10:55:51 +0530 sandy wrote
>
>
>
> >Hi everybody
>
> >I have one query regarding the heat input.
> >If I am welding a joint with multipass, then I have diffrent heat
> >input for every pass depening on the parameters. now I want to know
> >which heat input shall be taken into consideration for the effect of
> >heat input on base metal, cauz every pass has its effect on base metal
> >and after every pass due to the previous heat input I am giving extra
> >heat in the base metal.
> >So I want to know should I take individual heat input or sum of all
> >heat input for getting the exact effect of Heat input on base metal.
>
> >Regards
> >Sandeep Kumar
>
> >--
> >To post to this group, send email to materials-welding@googlegroups.com
> >To unsubscribe from this group, send email to
>
> materials-welding+unsubscribe@googlegroups.com>For more options, visit this group's bolg at
>
> http://materials-welding.blogspot.com/>The views expressed/exchnaged in this group are members personel views
>
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
>
>
> <http://sigads.rediff.com/RealMedia/ads/click_nx.ads/www.rediffmail.com/
> signatureline.htm@Middle?>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com