Thursday, January 27, 2011

RE: [MW:9514] CS in place of LTCS

This is LTCS pressure vessel plates with minimum tensile strength 55 Ksi.

 

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ayaz Mahmood
Sent: Thursday, January 27, 2011 12:30 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9513] CS in place of LTCS

 

Dear All,

 

          Can anybody tell me the Material A516 Gr. 55 is C.S or LTCS?

Thank's,
 




REMEMBER ME IN UR PRAYERS !
*******(¨`·.·´¨) (¨`·.·´¨)********
********`·.¸(¨`·.·´¨)..·´*********
*********** `·.¸.·´************

                                  
Best Regards,
Ayaz Merhmood
FEDC Dept.
I-G-D HABSHAN-5 PROJECT
DESCON ENGINEERING
(UAE)
Mobile : +971-50-1926232
www.descon.com.pk

 

 


From: yogesh <yogeshandpini@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thu, January 27, 2011 10:22:53 AM
Subject: [MW:9512] CS in place of LTCS

Can we replace LTCS with CS if temperature minimum expexted is
-20DegC,process fluid;Coolwing water???

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...