Sunday, January 30, 2011

Re: [MW:9571] welding consumable for 34 CrMoNi6 material


Hi,

this is dissimilar material and now you have to go for welding by using
electrode of ERCuNi GTAW shielding gas Argon 99.99%, backing gas
Argon 99.99%

Dia (mm) 1.6 ¶ 2.0 ¶ 2.4 ¶
Polarity DCEN
Current Range(A) 50-70 ¶ 50-80 ¶ 60-90 ¶
Voltage Range(V) 18-22 ¶ 18-22 ¶ 18-22 ¶


On Sun, 30 Jan 2011 18:17:18 +0530 wrote
>Hi Guys ,

We have to weld A36 grade material with 34 NiCrMo6 , can anybody tell
me which electrode can be used for the same .
If somebody has welding parameters also then please share .


Best Regards ,-----------------Dinesh Tiwari








--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...