[MW:9597] Flattening Test for SA 106

Dear Experts,
 
Refer to Section 12.0(Flattening Test) of SA 106, ASME Sec II Part A.
This Section states that - " For Pipe over NPS 2 a section of pipe not less than........"
 
Question: Does the above Interpretation includes 2" or excludes 2" for the Flattening Test?
Do provide the reference of ASME/ASTM which supports the Interpretation.
 
The MTC recieved does not reflect the Flattening Test.( Material - 2", Sch 80, SA 106 Gr.B for Sour Service)
 
Hope to see as usual co-operation from everyone in Material Group.
 
Thanks & Regards
Vino P Varghese
Doha-Qatar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...