What's the applicable specification for this material, ASTM/ASME/EN or any proprietary grade for any client or any vendor's specification.The elongation and impact properties asked are highly un-realistic. You never get a Carbon or Low Alloy steel with 46% elongation requirement, also, impact requirement is extremely high.
 
I would say, if you have any design paper work, which indicates the grade or heat treatment of this steel the correct AWS type of welding consumables, SAW wire+flux specification  etc could be worked out. Otherwise YOU SHOULD NEVER CHOOSE WELDING CONSUMABLES BASED ON THE CHEMICAL COMPOSITION ALONE.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario, Canada.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pablo J Acelajado
Sent: Thursday, January 27, 2011 10:08 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:9529] Requirement of suitable welding consumables SAW and SMAW

 

January 27, 2011

 

Hello there!

 

This material is very strong one. I think the welding consumable suppliers can best answer this question.

My understanding is that the percentage elongation is not required for the weld.

Thank you.

 

Best regards.

PJA


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Thursday, January 27, 2011 1:10 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:9526] Requirement of suitable welding consumables SAW and SMAW

 

Hi

 

The elongation requirement is very stringent, it is very difficult to meet 46%, you have consult with the specific consumable suppliers to get 46%

 

Thanks & Regards,

 

K. Babu


----- Original Message -----

Sent: Thursday, January 27, 2011 4:36 PM

Subject: [MW:9523] Requirement of suitable welding consumables SAW and SMAW

 

Hi Friends,

Let me get your expertise of selection of welding consumables in this
regard.

The base material Chemical properties as given under (%):

C - 0.066
Si - 0.26
Mn - 1.55
P - 0.014
S - 0.004
Al - 0.046
Cr - 0.186
Ni - 0.015
Mo - 0.002
Cu - 0.020
V - 0.057
Nb - 0.065
Ti - 0.020
N - 0.007
B - 0.00025
Ca - 0.0025
CE - 0.371

MECHANICAL PROPERTIES
YIELD STRENGTH - 516 MPa
TENSILE STRENGTH - 625 MPa.
ELONG % - 46
IMOPACT - (-) 10 DEGREE C - 250 JOULES

NOW PLEASE TELL ME, WHICH ELECTRODE FOR SMAW (BRAMDS ESAB, OERLIKON)
AND SAW - FLUX AND WIRE WILL SUIT AND PASS PQR TEST FOR PREPARATION OF
WPS?

PLEASE HELP.
THANKING YOU.



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs