On Thu, Aug 19, 2010 at 2:30 PM, pravin dhoria <pravindhoria@gmail.com> wrote:
Dear Friends,
 
Can anyone suggest/guide me about the failure of adhesion between polyethylene and adhesive material while we do three layer polyethylene coating on M.S. coating.
(1st layer-fusion bonded epoxy powder,2nd layer-adhesive ,3rd layer-poly ethylene)
 
 
Regards,
 
Pravin V. Dhoria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...