[MW:6593] Welding procedure Thickness range qualification

Dear All

BY ASME Sec IX for Welder Thickness range qualification, I am
referring QW 403.8 thats tells tat refer QW 451.1.
but wats QW 403.6 says? If we refer QW 451.1 is correct or not?

If we see welding variables QW 403.8 is essential variable & QW 403.6
is supplementry variables. wat SEC IX says

For welder thickness range qualification wat we have to refer? either
403.8 or403.6 ?
Pl explain this?

Regards
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...