Re: [MW:6285] RE: 6250] clad welding


see attached file for better clarity.

On 2 August 2010 17:21, Potter, Richard <RPotter@itses.com> wrote:
The base material 516-70 should be masked back so that the cladding is
about 1/2" back from the edge of the bevel on both sides.
You would then weld the 516-70 to 516-70 under your normal conditions.
After the required NDE is completed you would restore the 410 cladding.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of lusky
Sent: Monday, August 02, 2010 6:44 AM
To: Materials & Welding
Subject: [MW:6250] clad welding

I have to weld SA516 Gr 70 which has a 410 clad backing has anybody
done this? if so how were the results, there is no PWHT involved. 25mm
thick plate for a pressure vessle.
I have to qualify a PQR would be interested to read all comments

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...