Thursday, February 4, 2010

Re: [MW:4214] Submerged ARC Welding Machine


Dear Paresh,

One suggestion ESAB Circotech A4/A6, supplied by ESAB, see www.esab.com

Regards,


Claes Gillenius
Development Engineer, MMA. (Spec. stainless and non Fe-alloys)
Direct tel:  +46 (0)31 509315
Mobile +46 (0)707532012
Company                ESAB AB
Address                  Box 8004, 402 77  Gothenburg, Sweden
                                 LindholmsallĂ©n 9
Company  reg number        556005-7738



PARESH PATEL <paresh_proj@hotmail.com>
Sent by: materials-welding@googlegroups.com

2010-02-04 17:19

Please respond to
materials-welding@googlegroups.com

To
Mat <materials-welding@googlegroups.com>
cc
Subject
[MW:4213] Submerged ARC Welding Machine





 
Dear  Sir,
 
Pl. suggest   brand  name & supplier  for   Submerged ARC Welding   unit   to  use   vertical ( 2G Position )  seam welding  of  tanks.
 
Regards,
Paresh

 


Hotmail: Free, trusted and rich email service. Get it now.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This communication and any files transmitted with it contain information which is confidential and which may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient(s), please note that any disclosure, copying, printing or use whatsoever of this communication or the information contained in it is strictly prohibited. If you have received this communication in error, please notify us by e-mail or by telephone as above and then delete the e-mail together with any copies of it. ESAB does not accept liability for the integrity of this message or for any changes, which may occur in transmission due to network, machine or software failure or manufacture or operator error. Although this communication and any files transmitted with it are believed to be free of any virus or any other defect which might affect any computer or IT system into which they are received and opened, it is the responsibility of the recipient to ensure that they are virus free and no responsibility will be accepted by ESAB for any loss or damage arising in any way from receipt or use thereof.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...